# item.guide
Side-by-Side Comparison Battery Chemistries

Lead-Acid (AGM / Gel / Flooded) vs. Nickel-Cadmium (NiCd)

Comparing 2 standards across 9 specifications. 9 key differences identified.

Comparing:
Lead-Acid (AGM / Gel / Flooded)
Nickel-Cadmium (NiCd)

Lead-Acid is the oldest rechargeable battery chemistry (invented 1859), delivering 2.0V per cell (12V nominal in standard 6-cell monoblocs). Despite low gravimetric energy density (30–50 Wh/kg), its unmatched surge current delivery (hundreds of cold cranking amps), low production cost, and 99% recycling rate make it the universal standard for automotive starting/ignition (SLI) and industrial UPS systems.

View full Lead-Acid (AGM / Gel / Flooded) spec sheet →

Nickel-Cadmium (NiCd) is a mature, exceptionally rugged alkaline secondary chemistry operating at 1.2V nominal. Renowned for sustaining massive pulse discharge currents, operating reliably in deep sub-zero temperatures (-40°C), and enduring harsh electrical abuse, NiCd remains in service for aircraft backup power, emergency lighting, and legacy industrial systems.

View full Nickel-Cadmium (NiCd) spec sheet →

Specification Comparison Table

9 Parameters
Parameter / Spec
Nominal Cell Voltage
2.00 (12.00 V 6-Cell Pack) V 1.20 V
Gravimetric Energy Density
30 – 50 Wh/kg 45 – 65 Wh/kg
Volumetric Energy Density
60 – 100 Wh/L 120 – 160 Wh/L
Cycle Life (to 80% Capacity)
300 – 1,000 (Deep Cycle AGM) Cycles 1,000 – 2,000 Cycles
Thermal Runaway Threshold
> 200 °C > 260 °C
Operating Temperature Range
-20 to +50 °C -40 to +60 °C
Self-Discharge Rate
3 – 5% / Month 15 – 20% / Month
Primary Anode Material
Porous Sponge Lead (Pb) Metallic Cadmium (Cd)
Primary Cathode Material
Lead Dioxide (PbO2) in Sulfuric Acid Electrolyte (H2SO4) Nickel Oxyhydroxide (NiOOH)